Multifunctional Ni/NiO hybrid nanomembranes as anode materials for high-rate Li-ion batteries
X Sun, W Si, X Liu, J Deng, L Xi, L Liu, C Yan, OG Schmidt
Nano Energy 9, 168-175, 2014
2492014
High-defect hydrophilic carbon cuboids anchored with Co/CoO nanoparticles as highly efficient and ultra-stable lithium-ion battery anodes
X Sun, GP Hao, X Lu, L Xi, B Liu, W Si, C Ma, Q Liu, Q Zhang, S Kaskel, ...
Journal of Materials Chemistry A 4 (26), 10166-10173, 2016
1512016
Hierarchically designed SiOx/SiOy bilayer nanomembranes as stable anodes for lithium ion batteries
L Zhang, J Deng, L Liu, W Si, S Oswald, L Xi, M Kundu, G Ma, T Gemming, ...
Advanced materials 26 (26), 4527-4532, 2014
1322014
Sandwich nanoarchitecture of Si/reduced graphene oxide bilayer nanomembranes for Li-ion batteries with long cycle life
X Liu, J Zhang, W Si, L Xi, B Eichler, C Yan, OG Schmidt
ACS nano 9 (2), 1198-1205, 2015
1302015
High-rate amorphous SnO 2 nanomembrane anodes for Li-ion batteries with a long cycling life
X Liu, J Zhang, W Si, L Xi, S Oswald, C Yan, OG Schmidt
Nanoscale 7 (1), 282-288, 2015
682015
In Situ‐Formed, Amorphous, Oxygen‐Enabled Germanium Anode with Robust Cycle Life for Reversible Lithium Storage
X Sun, W Si, L Xi, B Liu, X Liu, C Yan, OG Schmidt
ChemElectroChem, 737-742, 2015
492015
High-temperature wetting and interfacial interaction between liquid Al and TiB 2 ceramic
L Xi, I Kaban, R Nowak, B Korpała, G Bruzda, N Sobczak, N Mattern, ...
Journal of Materials Science 50 (7), 2682-2690, 2015
412015
High areal capacity, micrometer-scale amorphous Si film anode based on nanostructured Cu foil for Li-ion batteries
W Si, X Sun, X Liu, L Xi, Y Jia, C Yan, OG Schmidt
Journal of Power Sources 267, 629-634, 2014
312014
Hierarchically porous Pd/NiO nanomembranes as cathode catalysts in Li-O2 batteries
X Lu, Y Yin, L Zhang, L Xi, S Oswald, J Deng, OG Schmidt
Nano Energy 30, 69-76, 2016
292016
Curly MnOx nanomembranes as cathode materials for rechargeable lithium–oxygen battery systems
X Lu, W Si, X Sun, J Deng, L Xi, B Liu, C Yan, OG Schmidt
Journal of Power Sources 295, 197-202, 2015
182015
Microstructural characterization of graphite/CuCrZr joints brazed with CuTiH2Ni-based fillers
Y Mao, L Peng, S Wang, L Xi
Journal of Alloys and Compounds 716, 81-87, 2017
152017
Microstructural and mechanical characterizations of W/CuCrZr and W/steel joints brazed with Cu-22TiH2 filler
L Peng, Y Mao, Y Zhang, L Xi, Q Deng, G Wang
Journal of Materials Processing Technology 254, 346-352, 2018
122018
Wetting, reactivity, and phase formation at interfaces between Ni–Al melts and TiB2 ultrahigh‐temperature ceramic
L Xi, I Kaban, R Nowak, G Bruzda, N Sobczak, J Eckert
Journal of the American Ceramic Society 101 (2), 911-918, 2018
102018
Wetting behavior and interfacial interactions of molten Cu50Ti alloy with hexagonal BN and TiB2 ceramics
Y Mao, L Peng, Q Deng, D Nie, S Wang, L Xi
Ceramics International 42 (8), 9906-9912, 2016
92016
Joining of tungsten to CuCrZr alloy with Cu-TiH2-Ni filler and Cu interlayer
S Peng, Y Mao, M Min, L Xi, Q Deng, G Wang, S Wang
International Journal of Refractory Metals and Hard Materials 79, 31-36, 2019
82019
Investigation of Ni-B alloys for joining of TiB 2 ultra-high-temperature ceramic
L Xi, I Kaban, R Nowak, G Bruzda, N Sobczak, M Stoica, J Eckert
Journal of Materials Engineering and Performance 25 (8), 3204-3210, 2016
82016
Wettability and work of adhesion of liquid sulfur on carbon materials for electrical energy storage applications
I Kaban, R Nowak, G Bruzda, L Xi, N Sobczak, J Eckert, L Giebeler
Carbon 98, 702-707, 2016
82016
Interfacial interactions between liquid Ti–Al alloys and TiB2 ceramic
L Xi, I Kaban, R Nowak, G Bruzda, N Sobczak, J Eckert
Journal of materials science 51 (4), 1779-1787, 2016
82016
纳米复合相变材料
席丽霞, 金学军
热加工工艺 41 (14), 5-9, 2012
82012
Wettability and Reactivity of ZrB 2 Substrates with Liquid Al
R Nowak, N Sobczak, G Bruzda, J Wojewoda-Budka, ...
Journal of Materials Engineering and Performance 25 (8), 3310-3316, 2016
52016