Chemical and thermal shrinkage in thermosetting prepreg OG Kravchenko, SG Kravchenko, RB Pipes Composites Part A: Applied Science and Manufacturing 80, 72-81, 2016 | 103 | 2016 |
Prediction of the chemical and thermal shrinkage in a thermoset polymer OG Kravchenko, C Li, A Strachan, SG Kravchenko, RB Pipes Composites Part A: Applied Science and Manufacturing 66, 35-43, 2014 | 87 | 2014 |
Digital image correlation measurement of resin chemical and thermal shrinkage after gelation OG Kravchenko, SG Kravchenko, A Casares, RB Pipes Journal of Materials Science 50, 5244-5252, 2015 | 70 | 2015 |
Cure history dependence of residual deformation in a thermosetting laminate OG Kravchenko, SG Kravchenko, RB Pipes Composites Part A: Applied Science and Manufacturing 99, 186-197, 2017 | 61 | 2017 |
Effect of curing rate on the microstructure and macroscopic properties of epoxy fiberglass composites A Patel, O Kravchenko, I Manas-Zloczower Polymers 10 (2), 125, 2018 | 38 | 2018 |
Composite toughness enhancement with interlaminar reinforcement S Kravchenko, O Kravchenko, M Wortmann, M Pietrek, P Horst, RB Pipes Composites Part A: Applied Science and Manufacturing 54, 98-106, 2013 | 37 | 2013 |
Effect of polycarbonate film surface morphology and oxygen plasma treatment on mode I and II fracture toughness of interleaved composite laminates X Qian, OG Kravchenko, D Pedrazzoli, I Manas-Zloczower Composites Part A: Applied Science and Manufacturing 105, 138-149, 2018 | 35 | 2018 |
A two-parameter fracture mechanics model for fatigue crack growth in brittle materials SG Kravchenko, OG Kravchenko, CT Sun Engineering Fracture Mechanics 119, 132-147, 2014 | 34 | 2014 |
Interlaminar stresses in composite laminates subjected to anticlastic bending deformation J Goodsell, NJ Pagano, O Kravchenko, R Byron Pipes Journal of Applied Mechanics 80 (4), 041020, 2013 | 33 | 2013 |
Role of annealing and isostatic compaction on mechanical properties of 3D printed short glass fiber nylon composites PAK Jain, S Sattar, D Mulqueen, D Pedrazzoli, SG Kravchenko, ... Additive Manufacturing 51, 102599, 2022 | 32 | 2022 |
Design and formulation of a completely biobased epoxy structural adhesive A Patel, S Mekala, OG Kravchenko, T Yilmaz, D Yuan, L Yue, RA Gross, ... ACS sustainable chemistry & engineering 7 (19), 16382-16391, 2019 | 29 | 2019 |
Phase field modeling of damage in glassy polymers Y Xie, OG Kravchenko, RB Pipes, M Koslowski Journal of the Mechanics and Physics of Solids 93, 182-197, 2016 | 28 | 2016 |
Incorporation of plasma-functionalized carbon nanostructures in composite laminates for interlaminar reinforcement and delamination crack monitoring OG Kravchenko, D Pedrazzoli, D Kovtun, X Qian, I Manas-Zloczower Journal of Physics and Chemistry of Solids 112, 163-170, 2018 | 27 | 2018 |
Conductive interlaminar interfaces for structural health monitoring in composite laminates under fatigue loading OG Kravchenko, D Pedrazzoli, VS Bonab, I Manas-Zloczower Materials & Design 160, 1217-1225, 2018 | 24 | 2018 |
Thickness dependence of mode I interlaminar fracture toughness in a carbon fiber thermosetting composite OG Kravchenko, SG Kravchenko, CT Sun Composite Structures 160, 538-546, 2017 | 21 | 2017 |
Mechanical behavior of long discontinuous glass fiber nylon composite produced by in-situ polymerization S Sattar, BB Laredo, D Pedrazzoli, M Zhang, SG Kravchenko, ... Composites Part A: Applied Science and Manufacturing 154, 106779, 2022 | 17 | 2022 |
An experimental investigation on low-velocity impact response and compression after impact of a stochastic, discontinuous prepreg tape composite SG Kravchenko, C Volle, OG Kravchenko Composites Part A: Applied Science and Manufacturing 149, 106524, 2021 | 17 | 2021 |
Modeling compressive behavior of open-cell polymerized high internal phase emulsions: effects of density and morphology OG Kravchenko, G Gedler, SG Kravchenko, DL Feke, I Manas-Zloczower Soft Matter 14 (9), 1637-1646, 2018 | 16 | 2018 |
Role of hierarchical morphology of helical carbon nanotube bundles on thermal expansion of polymer nanocomposites OG Kravchenko, X Qian, SG Kravchenko, R Misiego, RB Pipes, ... Journal of Materials Research 32 (14), 2738-2746, 2017 | 16 | 2017 |
Influence of through-thickness reinforcement aspect ratio on mode I delamination fracture resistance SG Kravchenko, OG Kravchenko, LA Carlsson, RB Pipes Composite Structures 125, 13-22, 2015 | 16 | 2015 |